模具skh51十堰材料供应商

    模具skh51十堰材料供应商

  购买时可以参考相关价格表,但这只是特定时间内的价格情况,价格会有波动,具体购买以实际成本为准。SKH51属高速钢日本的JIS品牌相当于德国的DIN 1.3343和美国的M2。

  SKH51高速钢

  Mn0.150.40

  Si0.20.45

  Cr3.804.4

  Mo4.55.5

  V1.752.2

  Skh51棒

  W5.56.75

  P≤0.030

  S≤0.030

  镍≤0.3

  铜≤0.25

  红硬性高,耐磨性高,切削能力强,冲击韧性高,晶粒细小均匀,韧性高。SKH-51模具钢材料为钨钢制成的高速钢,适用于制造强力切削的耐磨抗冲击刀具,模具和螺丝模具,韧性和形状复杂的刀具,铣刀模具skh51,钻头等。

  ①W-MO系列(6-5-2型)高速工具钢更为常见,尤其是SKH51,在国际上被广泛用于替代W型高速工具钢SKH2。

  ②碳化物组织细小、整齐、分布均匀。而且组织是统一的。所以耐磨性和韧性比较平衡。特别是,因为只有碳含量增加或减少,高温特性没有被破坏,钢的性能可以连续地和大幅度地改变。需要韧性时适合低碳钢,需要硬度和耐磨性时适合高碳钢钟表。

  (3)具有丰富的热加工和冷加工塑性,具有良好的切削性和磨削性。

  工具行业:刮刀、滚刀、铣刀、钻头等。

  锻造工业:锻模

  螺丝行业:六角平头成型模skh51板牙、丝锥、冲头。

  热处理温度和参考方法:

  退火:温度为℃,以1020℃/小时的速度随炉冷却至600℃左右,硬度在HB269以下;

  预热1:温度℃每隔25 mm保持30分钟。

  预热2:温度℃,每1毫米保温2030秒

  每1mm预热3:0℃2030秒,适用于大型复杂工件。

  奥氏体化:温度℃,每1毫米1015秒。

  淬火介质:油、热浴、空气或气体;

  温度℃,每25毫米60分钟以上,回火次数3次以上,硬度HRC64以上。

  一般中碳钢不使用skh51作为模具的主材,只作为附属材料。

  模具的顶杆一般采用碳素工具钢,如T10A钢。值得注意的是,采用盐油双液淬火时弯曲变形较大。要用三种方法使顶杆硬度达到53-58 HRC,可以减少顶杆的弯曲变形。

  规格/毫米

  盘条高速钢

  Ф5.5-30

  SKH51

  冷拉圆高速钢

  Ф3.0-100

  SKH51

  Ф3.0-350

  SKH51

  高速钢钢鼓乐队

  0.1-5.010-1000

  SKH51

  高速钢热轧圆钢

  Ф14-350

  SKH51

  高速钢hot rolled sheet

  1-180

  SKH51

  高速钢cold-rolled plate

  0.1-4.

  SKH51

  0.1-180

  SKH51

  Also known as Fenggang or Fenggang, it means that when quenched, it can be hardened even if it is cooled in air, and it is very sharp. It is a kind of alloy steel with complex composition, which contains carbide forming elements such as tungsten, molybdenum, chromium, vanadium and cobalt. The total amount of alloying elements is about 10 ~ 25%. It can still maintain high hardness under the condition of high heat caused by high-speed cutting (about 500℃), and the HRC can be above 60. this is高速钢The main characteristic is red hardness. Although carbon tool steel has a high hardness at room temperature after quenching and tempering at low temperature, when the temperature is higher than 200℃, the hardness drops sharply, and at 500℃, the hardness is similar to that of annealed state, and the ability to cut metal is completely lost, which limits the use of carbon tool steel for making cutting tools. but高速钢由于其良好的红色硬度, 它弥补了碳素工具钢的致命缺点,可用于制造切削工具。

  查看相关信息> >苏州东锜精密模具材料有限公司是一家专业从事国内外知名专业的公司模具钢材料销售、大型铣床研磨板加工、真空热处理于一体的模具企业,公司综合实力雄厚,技术设备精良,配套设施齐全;并拥有一批技术精湛的工程师和一支经验丰富的售后服务队伍,严格的质量管理体系和科学严谨的管理机制。

本文部分内容来源于网络,我们仅作为信息分享。本站仅提供信息存储空间服务,不拥有所有权,不承担相关法律责任。如发现本站有涉嫌抄袭侵权/违法违规的内容,请发送邮件至tokaits@163.com举报,一经查实,本站将立刻删除。

下一篇:pm60模具钢材哪里有硬度范围一览表
用手机扫描二维码关闭
Baidu
map